01Introduction
Peeling is the most visible coating failure.
Testing on the real substrate and primer system is more useful than testing on a clean steel panel only.
02Why It Matters
- Checks the system, not just the paint
- Shows surface preparation effect
- Supports data sheets
03Tests & Reference Methods
| Test | Purpose | Reference |
|---|---|---|
| Cross-cut tape | Rating of flaking on grid | Standard cross-cut method |
| Pull-off | Force to detach | Dolly and tester |
| Scratch and bend tests | Flexibility and bond | Panel tests |
| Water immersion adhesion | Wet adhesion | After soak |
04Reading the Results
| Observation | What it usually means | Action |
|---|---|---|
| Flaking at edges | Poor surface preparation | Improve cleaning and primer |
| Failure between coats | Incompatible or late recoat | Check recoat window |
| Failure at substrate | Weak surface or contamination | Better preparation |
| Cohesive failure in coating | Weak film | Reformulate |
05How IPCS Supports Your Laboratory
- Method selection
- Panel and system preparation
- Failure analysis
Methods and limits depend on your product and applicable standard. We confirm them with you before the laboratory is commissioned.
06Frequently Asked Questions
Which test is simplest?
Cross-cut with tape.
When to use pull-off?
For thick coatings, floors and waterproofing where force values matter.
What causes poor adhesion?
Dirty surface, wrong primer, early recoating or incompatible products.
Do I test after cure?
Yes, after full cure.
Can I test on site?
Pull-off can be done on site.