01Introduction
Non-shrink grouts are specification-driven products sold to contractors and industrial plants. Failure means a loose machine base, so buyers want data.
Accurate batching and a clean line are more important than machine size.
02What Is Non-Shrink Grout?
The grout needs to flow into tight spaces without bleeding or segregating, then expand slightly to remain in contact with the base plate, and then reach high early and final strength. Expansion can come from aluminium powder, calcium sulfoaluminate or other systems.
ASTM C1107 covers packaged dry hydraulic-cement grout (non-shrink), and other standards apply in other markets.
03Applications & End Uses
- Machine foundation base plates
- Anchor bolts and rebar fixing
- Precast joints and column bases
- Bridge bearings and structural repairs
04Types, Grades & Variants
| Type | Features | Use |
|---|---|---|
| Flowable cementitious grout | Pourable, high strength | Base plates |
| Pourable plastic grout | Stiffer, for larger gaps | Columns |
| Dry pack grout | Very stiff | Small gaps |
| Epoxy grout | Chemical resistance | Special foundations |
05Raw Materials & Their Functions
| Raw material | Function | Selection note |
|---|---|---|
| Cement (OPC or rapid) | Binder | Consistent, fresh |
| Graded fine sand (0 to 1 mm) | Aggregate | Narrow grading, dry |
| Expansion agent | Compensate shrinkage | Type and dose by trial |
| Powder superplasticiser (PCE, melamine) | Flow with low water | Efficiency and compatibility |
| Silica fume (optional) | Strength, cohesion | Dosing and handling |
| Defoamer, anti-bleed additives | Stability | Small doses |
06Formulation Guidance
Non-shrink grouts have low water demand and high cement plus fine aggregate content.
| Component group | Indicative range | Why it matters |
|---|---|---|
| Cement | 25% to 40% | Binder |
| Fine aggregate | 50% to 70% | Body |
| Expansion and plasticiser | 0.5% to 3% | Expansion, flow |
| Silica fume and others | 0% to 8% | Strength |
07Manufacturing Process
- Dry and screen aggregateVery low moisture.
- Pre-blend additivesSmall premix.
- Weigh accuratelyLow tolerance.
- MixRibbon or paddle mixer.
- Test flow and expansion
- PackMoisture-proof bags, small to 25 kg.
08Machinery & Equipment
| Machine | Role in this product |
|---|---|
| Ribbon Blender | Mixer |
| Powder Mixing & Dry Mortar Mixer | Powder mixer |
| Dry Mix Plant Machinery | Full line |
09Plant Layout, Space & Utilities
- Precise scales for additives
- Moisture-proof packing
- Testing cubes and flow cone
10Quality Control & Testing
| Test or check | What it tells you | Method or reference |
|---|---|---|
| Flow | Pourability | Flow cone or flow table |
| Expansion | Non-shrink behaviour | Height change method |
| Compressive strength | Early and 28-day | Cubes |
| Bleeding and segregation | Stability | Standard test |
| Initial and final set | Working time | Vicat |
11Common Production Problems & Fixes
| Problem | Likely cause | What to do |
|---|---|---|
| Bleeding | Water too high or no stabiliser | Adjust |
| Shrinkage cracks | Wrong expansion system | Re-formulate |
| Low flow | Plasticiser | Increase dose |
| Lumps | Moisture | Better packing |
| Strength lower than claim | Cement variation | Test cement |
12Capacity, Cost & Investment Factors
Quality, not volume, defines this product:
- Additive cost
- Testing equipment
- Technical sales
- Packaging
13How IPCS Supports This Project
- Formulation and test plan
- Specification data sheets
- Batching procedure
Scope, deliverables and timelines are written into a quotation after we understand your products, capacity, site and budget. Machine details are indicative and are finalised against your product.
14Frequently Asked Questions
What is non-shrink grout?
A grout that does not shrink and sometimes expands slightly so it stays in contact with the base plate.
What standards are used?
ASTM C1107 is one; check local specifications.
Is it easy to make?
The mixing is easy; accuracy and testing are the challenge.
Can I use it for anchor bolts?
Yes, with grades designed for it.
What is the shelf life?
Months in sealed bags.
How can IPCS help me start non-shrink grout manufacturing?
IPCS confirms the product range and capacity, plans the process and machines, tunes the formulation with your raw materials, sets up the laboratory, trains your team and supports the first batches. The written quote states exactly what is included.