01Introduction
Drying time affects recoat schedules and customer satisfaction.
Claims on the label should come from tests in stated conditions.
02Why It Matters
- Backs up label claims
- Controls solvent or driers balance
- Sets recoat intervals
03How the Test or Routine Works
- Apply filmFixed thickness.
- Control conditionsTemperature and humidity logged.
- Check surface dryLight touch.
- Check tack-freeCotton test.
- Check hard dryThumb or standard test.
- Record timesWith conditions.
04How IPCS Supports Your Laboratory
- Standard test conditions
- Data sheet wording
- Adjustment of formulation
Methods and limits depend on your product and applicable standard. We confirm them with you before the laboratory is commissioned.
05Frequently Asked Questions
What affects drying time?
Temperature, humidity, film thickness, airflow and formulation.
How do I test hard dry?
Thumb twist or per standard method.
What recoat time do I state?
Based on tests in typical conditions.
Why is film slow to dry?
Excess thickness, low temperature or wrong driers in enamels.
Do water paints dry the same way?
They dry by water loss and film formation, then cure further.