01Introduction
Cementitious waterproofing is the standard choice for bathrooms, sunken slabs, basements and tanks because it bonds to concrete, breathes and tolerates immersion when designed for it.
It sits between paint and dry mix mortar, which makes it a natural product for plants that already produce tile adhesive or putty.
02What Is Cementitious Waterproof Coating?
The slurry contains cement, graded fine sand or filler, polymer additives and sometimes crystalline or hydrophobic additives. Rigid single-pack types are mixed with water; flexible two-pack types are mixed with an acrylic or SBR liquid.
Flexible grades can bridge fine cracks, while rigid grades are used where there is no movement.
03Applications & End Uses
- Bathrooms and toilet floors under tiles
- Basements and sunken slabs
- Water tanks and sumps (rated grades)
- Swimming pools and planters (suitable grades)
- Retaining walls
04Types, Grades & Variants
| Type | Features | Use |
|---|---|---|
| Rigid one-pack | Cement, sand, additives; mix with water | Basements, retaining walls |
| Flexible two-pack | Powder plus liquid polymer | Bathrooms, terraces, tanks |
| Crystalline-type | Pore-blocking additives | Concrete structures |
| Under-tile waterproofing | Flexible and tile-adhesive compatible | Wet areas |
05Raw Materials & Their Functions
| Raw material | Function | Selection note |
|---|---|---|
| Portland cement (grey or white) | Binder | Fresh, consistent strength |
| Fine graded sand or filler | Body and shrinkage control | Dry, narrow grading |
| Redispersible polymer powder or liquid polymer | Flexibility and adhesion | Choose by flexibility class |
| Hydrophobic and crystalline additives | Water resistance | Dose by trial |
| Cellulose ether, defoamer | Workability | Small dose |
| Fibres (optional) | Crack control | Disperse evenly |
06Formulation Guidance
Formulas depend on class. Flexible two-pack products use a higher polymer content in the liquid component.
| Component group | Indicative range | Why it matters |
|---|---|---|
| Cement | 30% to 50% | Binder |
| Fine sand / filler | 40% to 60% | Body |
| Polymer powder (one-pack) | 2% to 12% | Flexibility |
| Additives | 0.5% to 4% | Workability, water repellency |
07Manufacturing Process
- Dry and screen sandMoisture control.
- WeighCement, sand and additives.
- Pre-blend additivesSmall premix.
- Main mixRibbon or paddle mixer.
- TestWorkability, setting, adhesion.
- PackMoisture-proof bags; liquid in pails.
08Machinery & Equipment
| Machine | Role in this product |
|---|---|
| Ribbon Blender | Main powder mixer |
| Powder Mixing & Dry Mortar Mixer | Powder mixing and screw feeding |
| Dry Mix Plant Machinery | Complete line with silos |
| Paint Filling Machine | Liquid polymer filling |
09Plant Layout, Space & Utilities
- Dry, enclosed building
- Dust collector and PPE
- Moisture-proof packaging
- Test bench with cube moulds and a water column
10Quality Control & Testing
| Test or check | What it tells you | Method or reference |
|---|---|---|
| Workability and pot life | Application | Flow test and timing |
| Water impermeability | Waterproofing | Water pressure test on cured samples |
| Adhesion to concrete | Bond | Pull-off |
| Flexibility class | Crack bridging | Crack-bridging test |
| Setting time | Handling | Vicat |
11Common Production Problems & Fixes
| Problem | Likely cause | What to do |
|---|---|---|
| Cracks after drying | Rigid grade on moving slab | Use flexible grade |
| Pinholes | Air entrapment | Better mixing and application |
| Weak adhesion | Contaminated substrate | Surface cleaning |
| Short pot life | Hot weather | Add retarder, mix small batches |
| Powder lumps | Moisture ingress | Better packing |
12Capacity, Cost & Investment Factors
Cost mainly reflects polymer content and packaging:
- Polymer powder or liquid cost
- Cement price
- Two-pack kit packaging
- Dealer and applicator training
13How IPCS Supports This Project
- Formulation by flexibility class
- Plant layout for dust control
- Test plan for waterproofing claims
Scope, deliverables and timelines are written into a quotation after we understand your products, capacity, site and budget. Machine details are indicative and are finalised against your product.
14Frequently Asked Questions
Is cementitious coating better than acrylic?
They serve different needs. Cementitious coatings are better for wet areas and immersion; acrylics are better for flexible roof coatings.
Can it be applied under tiles?
Yes, flexible under-tile grades are made for it. Confirm compatibility with the tile adhesive.
What is a two-pack system?
A powder component mixed on site with a liquid polymer component.
How is it cured?
Keep it damp for the period in the data sheet.
Can I make it in a tile adhesive plant?
Yes, with separate batching and cleaning between products. See tile adhesive plant.
How can IPCS help me start cementitious waterproof coating manufacturing?
IPCS confirms the product range and capacity, plans the process and machines, tunes the formulation with your raw materials, sets up the laboratory, trains your team and supports the first batches. The written quote states exactly what is included.